Optimization of Plasma Sparay Coating Parameters of Alumina Ceramic by Taguchi Experimental Method
이형근, 김대훈, 윤충섭


Correspondence:   Published online December 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
661
View
0
Download
Related articles
Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method  2018 February;36(1)
A Study on the Optimization of IR Laser Flip-chip Bonding Process Using Taguchi Methods  2008 June;26(3)
Optimization of the Plasma Spray Coating Parameters of Ni-5%AI Alloy Powder   2002 October;20(5)
Optimization of HVOF Spray Parameters for Cr3C2-7wt%NiCr Coating Powder by Experimental Design Method   1997 February;15(1)
Plasma Spray Coating of Zirconia Ceramic   1989 June;7(2)
Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method  2018 February;36(1)
A Study on the Optimization of IR Laser Flip-chip Bonding Process Using Taguchi Methods  2008 June;26(3)
Optimization of the Plasma Spray Coating Parameters of Ni-5%AI Alloy Powder   2002 October;20(5)
Optimization of HVOF Spray Parameters for Cr3C2-7wt%NiCr Coating Powder by Experimental Design Method   1997 February;15(1)
Plasma Spray Coating of Zirconia Ceramic   1989 June;7(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.