Effect of Heat Treatment on the Microstructures and Properties of HVOF Sprayed Ni-Cr-W-Mo-B Alloy Coatings
민경오, 이창희

Correspondence:   Published online December 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
933
View
0
Download
Related articles
The Effects of Heat Treatment Temperature on Wear Characteristics of Hyper-Eutectic Al-Si Alloy Laser Clad Layer  2019 June;37(3)
The Effect of Heat Treatment on Microstructure and Mechanical Behaviors of Laser Direct Energy Deposited Ti-6Al-4V Plate  2018 October;36(5)
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   2017 August;35(4)
Effect of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of P-No. 1 Carbon Steels  2017 February;35(1)
Effects of Post Weld Heat Treatment on Microstructures of Alloy 617 and 263 Welds for Turbines of HSC Power Plants  2016 June;34(3)
The Effects of Heat Treatment Temperature on Wear Characteristics of Hyper-Eutectic Al-Si Alloy Laser Clad Layer  2019 June;37(3)
The Effect of Heat Treatment on Microstructure and Mechanical Behaviors of Laser Direct Energy Deposited Ti-6Al-4V Plate  2018 October;36(5)
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   2017 August;35(4)
Effect of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of P-No. 1 Carbon Steels  2017 February;35(1)
Effects of Post Weld Heat Treatment on Microstructures of Alloy 617 and 263 Welds for Turbines of HSC Power Plants  2016 June;34(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.