Analysis on the Fatigue Crack Propagation of Weld Toe Crack through Residual Stress Field
김유일, 전유철, 강중규, 한종만, 한민구




Correspondence:   Published online October 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
642
View
0
Download
Related articles
Brittle Crack Propagation Path Due to the Effect of Welding Residual Stresses  2018 December;36(6)
Fatigue Crack Propagation Life Assessment of T-joint Fillet Weldment Considering Residual Stress under Random Loading  2011 April;29(2)
Numerical Analysis Model for Fatigue Life Prediction of Welded Structures  2009 December;27(6)
Analysis of Fatigue Durability on Seam Weldment using Notch Stress Approach  2004 April;22(2)
An Analysis of the Redistribution of Residual Stress Due to Crack Propagation Initially Through Residual Tensile Stress Field by Finite Element Method  2003 December;21(7)
Brittle Crack Propagation Path Due to the Effect of Welding Residual Stresses  2018 December;36(6)
Fatigue Crack Propagation Life Assessment of T-joint Fillet Weldment Considering Residual Stress under Random Loading  2011 April;29(2)
Numerical Analysis Model for Fatigue Life Prediction of Welded Structures  2009 December;27(6)
Analysis of Fatigue Durability on Seam Weldment using Notch Stress Approach  2004 April;22(2)
An Analysis of the Redistribution of Residual Stress Due to Crack Propagation Initially Through Residual Tensile Stress Field by Finite Element Method  2003 December;21(7)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.