Journal of KWJS 2000 August;18(4) :96-103.
Published online August 25, 2000.
Effect of Bonding Condition on High Temperature Mechanical Properties of TLP Bonded Joints of Fe-35Ni-26Cr Alloy
김대업
Correspondence:   Published online August 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
679
View
0
Download
Related articles
Effect of Sintering Conditions on Microstructure and Mechanical Strength of Cu Micro-Particle Sintered Joints for High-Power Semiconductor Module Applications  2019 April;37(2)
Effects of High Temperature-moisture on Corrosion and Mechanical Properties for Sn-system Solder Joints   2017 June;35(3)
Effects of Brazing Current on Mechanical Properties of Gas Metal Arc Brazed Joint of 1000MPa Grade DP Steels  2017 April;35(2)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures  2015 October;33(5)
Effect of Sintering Conditions on Microstructure and Mechanical Strength of Cu Micro-Particle Sintered Joints for High-Power Semiconductor Module Applications  2019 April;37(2)
Effects of High Temperature-moisture on Corrosion and Mechanical Properties for Sn-system Solder Joints   2017 June;35(3)
Effects of Brazing Current on Mechanical Properties of Gas Metal Arc Brazed Joint of 1000MPa Grade DP Steels  2017 April;35(2)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures  2015 October;33(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.