Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on Corrosion Failure of a Weathering Steel Weldment with Various Applied Potentials in Acid-chloride Solution

Journal of KWJS 2000;18(3):97-105.
Published online June 26, 2000.
산-염소이온 분위기의 인가전위에 따른 내후성강 용접부의 부식파괴에 관한 연구
, , ,
 
A Study on Corrosion Failure of a Weathering Steel Weldment with Various Applied Potentials in Acid-chloride Solution
최윤석, 김정구, 김종집, 이병훈