The Study on Microstructures and Mechasnical Properties of Mild Steel Joined with Various Spot Welding Conditions
강연철, 김대영, 김완기, 김석원



Correspondence:   Published online February 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
738
View
0
Download
Related articles
Intermetallic Compounds and Mechanical Property of Sn-Cu-xCr/Cu Solder Joint by Multiple reflows Conditions  2018 April;36(2)
Microstructure and Mechanical Properties in the Friction Stir Welded C70600 Alloy  2018 April;36(2)
Microstructure and Mechanical Properties of Gas Metal Arc Brazed Joint of DP Steel with Cu-Si Filler Metal  2016 October;34(5)
Analysis of Microstructure and Mechanical Properties According to Heat Treatment Conditions in GMAW for Al 6061-T6 Alloy  2016 August;34(4)
Correlation of Microstructure and Tribological Properties of Mo Blended Fe-Base Coatings Fabricated by Atmospheric Plasma Spraying  2014 October;32(5)
Intermetallic Compounds and Mechanical Property of Sn-Cu-xCr/Cu Solder Joint by Multiple reflows Conditions  2018 April;36(2)
Microstructure and Mechanical Properties in the Friction Stir Welded C70600 Alloy  2018 April;36(2)
Microstructure and Mechanical Properties of Gas Metal Arc Brazed Joint of DP Steel with Cu-Si Filler Metal  2016 October;34(5)
Analysis of Microstructure and Mechanical Properties According to Heat Treatment Conditions in GMAW for Al 6061-T6 Alloy  2016 August;34(4)
Correlation of Microstructure and Tribological Properties of Mo Blended Fe-Base Coatings Fabricated by Atmospheric Plasma Spraying  2014 October;32(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.