Effects of Surface Depression on Pool Convection and Oscillation in GTAW
고성훈, 최상균, 유중돈


Correspondence:   Published online December 27, 1999
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
617
View
0
Download
Related articles
Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S  2017 October;35(5)
Effects of the Support Condition on Out-of-plane Deformation by Welding   1999 October;17(5)
Effects of Initial Defects on Welding Deformation and Residual Stress   1999 August;17(4)
Effects of Wicking on solder Joint Profile in Gullwing Lead   1998 August;16(4)
Effects of Wire Speed Fluctuation on Arc Stability in GMA Welding   1995 December;13(4)
Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S  2017 October;35(5)
Effects of the Support Condition on Out-of-plane Deformation by Welding   1999 October;17(5)
Effects of Initial Defects on Welding Deformation and Residual Stress   1999 August;17(4)
Effects of Wicking on solder Joint Profile in Gullwing Lead   1998 August;16(4)
Effects of Wire Speed Fluctuation on Arc Stability in GMA Welding   1995 December;13(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.