Effects of cooling rate on Microstructure and Bond Strength in WC-Co / Cu / SM45C steel joint
정승부, 양훈모

Correspondence:   Published online April 26, 1999
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
673
View
0
Download
Related articles
Effect of Sintering Conditions on Microstructure and Mechanical Strength of Cu Micro-Particle Sintered Joints for High-Power Semiconductor Module Applications  2019 April;37(2)
Effects of Ni-P Bath on the Brittle Fracture of Sn-Ag-Cu Solder/ENEPIG Solder Joint   2017 June;35(3)
Effects of Post Weld Heat Treatment on Microstructures of Alloy 617 and 263 Welds for Turbines of HSC Power Plants  2016 June;34(3)
The Effects of Microstructure on Cold Crack in High-Strength Weld Metals  2014 February;32(1)
Effect of Coating Thickness on Microstructures and Tensile Properties in Yb:YAG Disk Laser Welds of Al-Si Coated Boron Steel  2013 June;31(3)
Effect of Sintering Conditions on Microstructure and Mechanical Strength of Cu Micro-Particle Sintered Joints for High-Power Semiconductor Module Applications  2019 April;37(2)
Effects of Ni-P Bath on the Brittle Fracture of Sn-Ag-Cu Solder/ENEPIG Solder Joint   2017 June;35(3)
Effects of Post Weld Heat Treatment on Microstructures of Alloy 617 and 263 Welds for Turbines of HSC Power Plants  2016 June;34(3)
The Effects of Microstructure on Cold Crack in High-Strength Weld Metals  2014 February;32(1)
Effect of Coating Thickness on Microstructures and Tensile Properties in Yb:YAG Disk Laser Welds of Al-Si Coated Boron Steel  2013 June;31(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.