Effects of Solidification Modes on the Pit Initiation and Propagation in Austenitic Stainless Steel Weld Metals
최한신, 김규영, 이창희


Correspondence:   Published online December 25, 1998
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
741
View
0
Download
Related articles
Effect of the Holding Time during Solution Heat Treatment on Intergranular Corrosion of Unstabilized Austenitic Stainless Steels  2020 June;38(3)
Effect of Composition on Strain-Induced Martensite Transformation and Tensile Stress-Strain Curve for Austenitic Stainless Steels  2018 April;36(2)
Effect of Restraint Stress on the Precipitation Behavior and Thermal Fatigue Properties of Simulated Weld Heat Affected Zone in Ferritic Stainless Steel  2015 December;33(6)
The Effect of Alloying Elements on Weldability and Corrosion Resistance of Austenitic Stainless Steels(I)  2012 June;30(3)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
Effect of the Holding Time during Solution Heat Treatment on Intergranular Corrosion of Unstabilized Austenitic Stainless Steels  2020 June;38(3)
Effect of Composition on Strain-Induced Martensite Transformation and Tensile Stress-Strain Curve for Austenitic Stainless Steels  2018 April;36(2)
Effect of Restraint Stress on the Precipitation Behavior and Thermal Fatigue Properties of Simulated Weld Heat Affected Zone in Ferritic Stainless Steel  2015 December;33(6)
The Effect of Alloying Elements on Weldability and Corrosion Resistance of Austenitic Stainless Steels(I)  2012 June;30(3)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.