The Effect of Current Pulsing Parameters on the Spatter Generation Rate during CO₂ Shielded Gas Metal Arc Welding
강덕일, 최재호, 장영섭, 김용석



Correspondence:   Published online August 25, 1998
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
630
View
0
Download
Related articles
Spatter Generation During Constant Voltage DC-AC Pulse Tandem Gas Metal Arc Welding Process  2018 June;36(3)
Effects of High Current and Welding Wire Diameter on the Magnesium Vaporization and Mechanical Properties of Al5083 Arc Welds  2013 December;31(6)
Effects of Welding Parameters on Porosity Formation in Weld Beads of Galvanized Steel Pipes produced with Gas Metal Arc Welding  2012 October;30(5)
The Effects of Process Parameters on Sealing Quality for Ir-192 Radiation Source Capsule using Resistance Spot Welding  2009 February;27(1)
The Eeffect of Arc Length and Shield Gas on Penetration Aspect Ratio in A-TIG Welding  2008 December;26(6)
Spatter Generation During Constant Voltage DC-AC Pulse Tandem Gas Metal Arc Welding Process  2018 June;36(3)
Effects of High Current and Welding Wire Diameter on the Magnesium Vaporization and Mechanical Properties of Al5083 Arc Welds  2013 December;31(6)
Effects of Welding Parameters on Porosity Formation in Weld Beads of Galvanized Steel Pipes produced with Gas Metal Arc Welding  2012 October;30(5)
The Effects of Process Parameters on Sealing Quality for Ir-192 Radiation Source Capsule using Resistance Spot Welding  2009 February;27(1)
The Eeffect of Arc Length and Shield Gas on Penetration Aspect Ratio in A-TIG Welding  2008 December;26(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.