A Study on the Fatigue Crack Growth Characteristics ofr the Weldment of Carbon steel-Stainless steel
권재도, 김우현, 김길수, 박중철, 배용덕, 김중형





Correspondence:   Published online August 25, 1998
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,031
View
0
Download
Related articles
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
Evaluation of Corrosion Characteristics According to Plastic Strain on Super Austenitic Stainless Steel(Base Metal)  2018 December;36(6)
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels  2018 October;36(5)
A Study on Fatigue Crack Growth Parameters for Fatigue Life Assessment based on Fracture Mechanics   2017 February;35(1)
A Study of Fatigue Crack Growth Behaviour for Ferrite-Bainite Dual Phase Steel  2016 February;34(1)
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
Evaluation of Corrosion Characteristics According to Plastic Strain on Super Austenitic Stainless Steel(Base Metal)  2018 December;36(6)
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels  2018 October;36(5)
A Study on Fatigue Crack Growth Parameters for Fatigue Life Assessment based on Fracture Mechanics   2017 February;35(1)
A Study of Fatigue Crack Growth Behaviour for Ferrite-Bainite Dual Phase Steel  2016 February;34(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI