Effect of Welding Residual Stress on Fatigue Crack Propagation Behavior
김응준
Correspondence:   Published online June 25, 1997
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
676
View
0
Download
Related articles
Effect of the welding residual stress redistribution on impact absorption energy  2015 February;33(1)
A Study on the Measurement of Stress Intensity Factors for the Fatigue Crack Propagation  2012 December;30(6)
Effect of Weld Residual Stress on Fatigue Analysis of Nozzle  2014 February;32(1)
Measurement of Welding Residual Stress in a 25-mm Thick Butt Joint using Inherent Strain Method  2013 August;31(4)
Redistributions of Welding Residual Stress for CTOD Specimen by Local Compression  2009 December;27(6)
Effect of the welding residual stress redistribution on impact absorption energy  2015 February;33(1)
A Study on the Measurement of Stress Intensity Factors for the Fatigue Crack Propagation  2012 December;30(6)
Effect of Weld Residual Stress on Fatigue Analysis of Nozzle  2014 February;32(1)
Measurement of Welding Residual Stress in a 25-mm Thick Butt Joint using Inherent Strain Method  2013 August;31(4)
Redistributions of Welding Residual Stress for CTOD Specimen by Local Compression  2009 December;27(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.