Advanced Search  
JWJ > Volume 15(1); 1997 > Article
Journal of KWJS 1997 February;15(1) :15-25.
Published online February 25, 1997.
Residual Stress , Distortion , and Fracture Analysis of Welded Structures using Finite Element Method
심용래
Correspondence:   Published online February 25, 1997
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
659
View
0
Download
Related articles
Welding Residual Stress Evaluation and Process Optimization of CTBA Trailing Arm using Finite Element Analysis  2018 August;36(4)
A weld-distortion analysis method of the shell structures using ultra structural FE model  2015 June;33(3)
A Study on the Thermal Distortion Analysis of Welded Structures having K/X Groove using shell elements  2012 December;30(6)
Residual Stress Prediction in Multi-layer Butt Weld Using Crack Compliance Method  2012 December;30(6)
Analysis of Weldment by Using Finite Element Method(1) - Heat Flow in Weldment -  2011 April;29(2)
Welding Residual Stress Evaluation and Process Optimization of CTBA Trailing Arm using Finite Element Analysis  2018 August;36(4)
A weld-distortion analysis method of the shell structures using ultra structural FE model  2015 June;33(3)
A Study on the Thermal Distortion Analysis of Welded Structures having K/X Groove using shell elements  2012 December;30(6)
Residual Stress Prediction in Multi-layer Butt Weld Using Crack Compliance Method  2012 December;30(6)
Analysis of Weldment by Using Finite Element Method(1) - Heat Flow in Weldment -  2011 April;29(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.