A Study on Mechanical Properties of Fillet Weldment in Pipeline Repair Welding Using Sleeve
김영표, 김형식, 김우식, 홍성호



Correspondence:   Published online October 25, 1996
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
903
View
0
Download
Related articles
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 December;37(6)
A Study on Process Robustness of Lap Joint Fillet Welding in GTAW Using C Type Filler  2019 October;37(5)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 August;37(4)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Mechanical Properties of Cu and Ni Dissimilar Welds by High Welding Speed Using Single-Mode Fiber Laser  2014 June;32(3)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 December;37(6)
A Study on Process Robustness of Lap Joint Fillet Welding in GTAW Using C Type Filler  2019 October;37(5)
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW  2019 August;37(4)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Mechanical Properties of Cu and Ni Dissimilar Welds by High Welding Speed Using Single-Mode Fiber Laser  2014 June;32(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.