Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Characteristics of Adhesive Bonded Joints of Steels for Automobile ( I )

Journal of KWJS 1995;13(2):106-114.
Published online June 26, 1995.
자동차용 강판의 접착특성 - 접착부의 접합강도와 영향인자 -
,
 
Characteristics of Adhesive Bonded Joints of Steels for Automobile ( I )