Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on the Fatigue Strength and Allowable Stress of INVAR ( Fe-36% Ni ) Steel Lap Joint Applied to Cargo Containment of LNG Carrier

Journal of KWJS 1994;12(1):102-115.
Published online March 25, 1994.
LNG선용 INVAR ( Fe-36%Ni ) 강 Lap 이음부의 피로강도와 허용응력에 관한 연구
, ,
 
A Study on the Fatigue Strength and Allowable Stress of INVAR ( Fe-36% Ni ) Steel Lap Joint Applied to Cargo Containment of LNG Carrier
한명수, 한종만, 한용섭