Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Microstructural Changes on Weld Heat Input in 60kg/mm2 Quenched and Tempered High Strength Steel

Journal of KWJS 1993;11(4):79-90.
Published online December 27, 1993.
60kg/mm2급 조질고장력강의 용접입열량에 따른 미세조직변화
, ,
 
Microstructural Changes on Weld Heat Input in 60kg/mm2 Quenched and Tempered High Strength Steel