Prediction of Penetration And Heat Affected Zone By Using Finite Element Method in CO2Arc Welding
이정익, 박일철, 박기영, 엄기원



Correspondence:   Published online December 25, 1992
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
689
View
0
Download
Related articles
Prediction of Plate Deformation by Multi-line Heating using SDB Method  2019 February;37(1)
Analysis of Weldment by Using Finite Element Method(1) - Heat Flow in Weldment -  2011 April;29(2)
Prediction of Nugget Shape by Finite Element Modeling in Arc-spot Welding   1999 April;17(2)
Prediction of Three-Dimensional Solder Joint Profile in Gullwing Lead using Finite Element Modeling   1998 August;16(4)
Prediction of Plate Deformation by Multi-line Heating using SDB Method  2019 February;37(1)
Analysis of Weldment by Using Finite Element Method(1) - Heat Flow in Weldment -  2011 April;29(2)
Prediction of Nugget Shape by Finite Element Modeling in Arc-spot Welding   1999 April;17(2)
Prediction of Three-Dimensional Solder Joint Profile in Gullwing Lead using Finite Element Modeling   1998 August;16(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.