A Study on the Development of Arc Sensor for Flux Cored Arc Welding Process and its Application for Seam Tracking
김수영, 이승영, 나석주


Correspondence:   Published online December 25, 1992
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
727
View
0
Download
Related articles
In-situ Strain Measurement of Submerged Arc Welding Process Through Application of Electronic Speckle Pattern Interferometry  2017 August;35(4)
A Study on Development of the Optimization Algorithms to Find the Seam Tracking  2016 April;34(2)
A Study on Development of STACO Model to Predict Bead Height in Tandem GMA Welding Process  2014 December;32(6)
A Study on the Measurement of Stress Intensity Factors for the Fatigue Crack Propagation  2012 December;30(6)
A Study of Weldability for Pure Titanium by Nd:YAG Laser(Ⅳ) - Lap Welding and Application for Heat Exchanger  2010 February;28(1)
In-situ Strain Measurement of Submerged Arc Welding Process Through Application of Electronic Speckle Pattern Interferometry  2017 August;35(4)
A Study on Development of the Optimization Algorithms to Find the Seam Tracking  2016 April;34(2)
A Study on Development of STACO Model to Predict Bead Height in Tandem GMA Welding Process  2014 December;32(6)
A Study on the Measurement of Stress Intensity Factors for the Fatigue Crack Propagation  2012 December;30(6)
A Study of Weldability for Pure Titanium by Nd:YAG Laser(Ⅳ) - Lap Welding and Application for Heat Exchanger  2010 February;28(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.