Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Study on the Hydrogen Embrittlement Crack Susceptibility of Stainless Steel Overlaid Weld Metal ( Report 1 )

Journal of KWJS 1990;8(3):39-52.
Published online September 25, 1990.
스테인레스강 Overlay용접부의 수소취화 균열감수성에 관한 연구 ( 1 )
 
Study on the Hydrogen Embrittlement Crack Susceptibility of Stainless Steel Overlaid Weld Metal ( Report 1 )