Effect of Sn and P on the Shear Strength of Copper to Stainless Steel Brazed Joint
정재필, 이보영, 이우천, 강춘식



Correspondence:   Published online September 25, 1989
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
884
View
0
Download
Related articles
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars  2019 February;37(1)
The Effect of PWHT on the Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW  2017 December;35(6)
Effects of Ni-P Bath on the Brittle Fracture of Sn-Ag-Cu Solder/ENEPIG Solder Joint   2017 June;35(3)
The Effect of Ti and Sn Contents on the Shear Bonding Strength of Brazing Joint of YSZ to STS430 using Ag Based Filler Metals  2014 February;32(1)
Effect of Curing Agent on the Curing Behavior and Joint Strength of Epoxy Adhesive  2011 August;29(4)
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars  2019 February;37(1)
The Effect of PWHT on the Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW  2017 December;35(6)
Effects of Ni-P Bath on the Brittle Fracture of Sn-Ag-Cu Solder/ENEPIG Solder Joint   2017 June;35(3)
The Effect of Ti and Sn Contents on the Shear Bonding Strength of Brazing Joint of YSZ to STS430 using Ag Based Filler Metals  2014 February;32(1)
Effect of Curing Agent on the Curing Behavior and Joint Strength of Epoxy Adhesive  2011 August;29(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.