Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on Pulse-GMA Welding of Al-7029 ( 1 ) - Influence of Welding Variables on The Weld Shape -

Journal of KWJS 1988;6(2):47-55.
Published online June 27, 1988.
AL-7029의 Pulse-GMA 용접에 관한 연구 ( 1 ) - 용접변수가 용접부형상에 미치는 영향 -
, , ,
 
A Study on Pulse-GMA Welding of Al-7029 ( 1 ) - Influence of Welding Variables on The Weld Shape -
김재웅, 허장욱, 나석주, 이용연