1. W.M. Thoms, E. D. Nicholas, J.C. Need Ham, and M. G. Murch, Friction stir butt welding:International patent application No. PCT/GB92/02203, GB patent application No. 9125978.8. (1991)
6. Y. M. Hwanga, Z. W. Kanga, YCH. Chioua, and H. H. Hsu, Experimental study on temperature distributions within the workpiece during friction stir welding of aluminum alloys,
International Journal of Machine Tools & Manufacture. 48 (2008) 778–787.
https://doi.org/10.1016/j.ijmachtools.2007.12.003
[CROSSREF]
9. R. Padmanaban, Kishore V. Ratna, and V. Balusamy, Numerical Simulation of Temperature Distribution and Material Flow During Friction Stir Welding of Dissimilar Aluminum Alloys,
Processing and Engineering. 97 (2014) 854–863.
https://doi.org/10.1016/j.proeng.2014.12.360
[CROSSREF]
11. A. Squillace, T. Segreto, U. Prisco, and G. Campanile, Optimization of Friction Stir Welds of Aluminium alloys,
IPROM. 135 (2006) 189–195.
[CROSSREF]
12. B. Donnetham and S. Watthanasikul, Comparison of the friction stir welding of aluminium alloy AA6063-T6 between cylindrical and rounded head, IE network conference. (2007)
13. K. Elangovan and V. Balasubramanian, Influences of tools pin profile and tool shoulder diameter on the formation of friction stir processing zone in AA6035 aluminium alloys,
Materials and Design. 29 (2008) 362–373.
https://doi.org/10.1016/j.matdes.2007.01.030
[CROSSREF]
14. M. Vural, A. Ogur, G. Cam, and C. Ozarpa, On the friction stir welding of aluminium alloys EN AW 2024-0 and EN AW 5754-H22, Material Science and Engineering A. 28 (2007) 49–54.
16. M. A. Sutton, A. P. Reynolds, D. Q. Wang, and C. R. Hubbard, A study of residual stresses and microstructure in 2024-T3 aluminum friction stir butt welds,
Journal of Engineering Materials and Technology ASME. 124(4) (2002) 215–221.
https://doi.org/101115/1.1429639
[CROSSREF] [PDF]
17. R. Keivani, B. Bagheri, F. Sharifi, M. Ketabchi, and M. Abbasi, Effects of pin angle and preheating on temperature distribution during friction stir welding operation“,
Transaction of. Nonferrous Metalls Society of China. 23 (2013) 2708–2713.
https://doi.org/10.1016/S1003-6326(13)62788-0
[CROSSREF]
19. M. Jafari, M. Abbasi, D. Poursina, A. Gheysarian, and B. Bagheri, Microstructures and mechanical properties of friction stir welded dissimilar steel-copper joints,
Journal Mechanical Science and Technoligy. 31(3) (2017) 11351142
https://doi.org/10.1007/s12206-016-1217-z
[CROSSREF] [PDF]
22. J. Zhang, Y. Shen, B. Li, H. Xu, X. Yao, B. Kuang, and J. Gao, Numerical simulation and experimental investigation on friction stir welding of 6061-T6 aluminum alloy,
Journal of Materials and Design. 60 (2014) 94–101.
https://doi.org/10.1016/j.matdes.2014.03.043
[CROSSREF]
25. ABAQUS/6.14.2. (2016), Providence, RI, USA: Dassault Systems Simulia Corp.
28. M. Abbasi, B. Bagheri, M. Dadaei, H. Omidvar, and M. Rezaei, The effect of FSP on mechanical, tribo-logical and corrosion behavior of composite layer developed on magnesium AZ91 alloy surface,
Inernational Journal Advanced Manufacturing and Technology. l77 (2015) 2051–2058.
https://doi.org/10.1007/s00170-014-6577-x
[CROSSREF] [PDF]
29. R. S. Mishra and Z. Y. Ma, Friction stir welding and processing,
Materials Science and Engineering R:Reports. 50 (2005) 1–78.
[CROSSREF] [PDF]
30. R. Kaibyshev, K. Shipilova, F. Musin, and Y. Motohashi, Continous dynamic recrystallization in an Al-Li-Mg-Sc alloy during equal-channel angular extrusion,
Material Science and Engineering A. 396 (2005) 341–351.
https://doi.org/10.1016/j.msea.2005.01.053
[CROSSREF]
31. D. Hull and D. J. Bacon. Introduction to dislocations. USA: Elsevier Ltd; 5th Ed. (2011), E-Book ISBN:9780080966731
32. W. D. Callister. Materials science and engineering:an introduction. Wiley; USA: (2007), ISNB:10:047173696-1
36. V. Uthaisangsuk. Microstructure based forma-bility modeling of multiphase steels. Ph.D. Thesis, IEHK, RWTH-Aachen. (2009)
38. M. Azizieh, R. Bahadori, M. Abbasi, E. Y. Yoon, and H. S. Kim, Effect of friction stir processing on the micro-structure of pure magnesium castings,
International Journal Casting Materials Research. 28 (2015) 345–351.
https://doi.org/10.1080/13640461.2015.1106780
[CROSSREF]
39. D. Ghanbari, Asgarani M. Kasiri, and K. Gharavi. Amini, Influence of heat treatment on mechanical properties and microstructure of the Al2024/SiC composite produced by multi-pass friction processing,
Measurement. 104 (2017) 151–158.
https://doi.org/10.1016/j.measurement.2017.03.024
[CROSSREF]
41. V. Bulatov and W. Cai. Computer Simulations of Dislocations.
Oxford Materials. 243-249 (2006), ISBN-13:978-0198526148
[CROSSREF]