Advanced Search  
JWJ > Volume 33(5); 2015 > Article
Journal of Welding and Joining 2015 October;33(5) :20-25.
Published online October 30, 2015.
doi:https://doi.org/10.5781/JWJ.2015.33.5.20
Clad Steel for Application of Hull Structure
Yong-Taek Shin*
*Dept. of Naval Architecture and Offshore Engineering, Dong-A University, Busan 656-710, Korea
Correspondence: Yong-Taek Shin  Email: ytshin@dau.ac.kr
  Published online October 30, 2015
ABSTRACT
Clad steel has good corrosion resistance and mechanical properties arising from the hot rolling of dissimilar metals, such as carbon steel and stainless steel. However both good corrosion resistance from the cladding plate material(stainless steel) and mechanical properties from the base plate material (carbon steel) are difficult to obtain because the different steels display opposite behaviors during the cladding process. In order to make clad steel for application in the hulls of ships, proper materials selection and heat-treatment conditions are necessary. In this study, mechanical properties of base plate materials with different chemical composition were evaluated according to heat condition of cladding plate material.
Keywords: Clad steel | Base plate materials | Super duplex stainless steel
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,074
View
6
Download
Related articles
Study on Joint of Micro Solder Bump for Application of Flexible Electronics  2013 June;31(3)
Trends of Welding Deformation Analysis for Ship Structure  2012 April;30(2)
Numerical Analysis Model for Fatigue Life Prediction of Welded Structures  2009 December;27(6)
Laser Application Group  2003 October;21(6)
A Study on Welding Deformation of I-Beam Steel Structure by FEM Method  2003 September;21(5)
Study on Joint of Micro Solder Bump for Application of Flexible Electronics  2013 June;31(3)
Trends of Welding Deformation Analysis for Ship Structure  2012 April;30(2)
Numerical Analysis Model for Fatigue Life Prediction of Welded Structures  2009 December;27(6)
Laser Application Group  2003 October;21(6)
A Study on Welding Deformation of I-Beam Steel Structure by FEM Method  2003 September;21(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.