A study on reduction of pre-crack deviation in CTOD specimen using reverse bending method
Sehwan Jeong**, Dong-Hwan Park*, Hyeon-su Kim**, Sang-beom Shin**, Tae-jong Park***
*Institute of e-Vehicle Technology, University of Ulsan, Ulsan 680-749, Korea
**Structure research department, Industrial Technology Institute, Hyundai Heavy Industry, Ulsan 682-792, Korea
***Materials research department, Industrial Technology Institute, Hyundai Heavy Industry, Ulsan 682-792, Korea
Correspondence: Dong-Hwan Park  Email: dhpark@ulsan.ac.kr
  Published online April 30, 2015
ABSTRACT
This study investigates the appropriate range of reverse bending load for the CTOD test of thick weld by observing improvement of pre-crack shape and determination of the limit applicable load. In order to do it, the effect of the amount of the reverse bending load on the maximum deviation of the pre-crack length was investigated by the extensive tests, and the variation of plastic zone size in way of the crack tip under reverse bending load were evaluated by FEA. With the results obtained by the experiments and FEA, the proper range of reverse bending load was suggested. The effectiveness of the reverse bending method was verified by examining the pre-crack straightness after CTOD tests of thick weld specimens with various thickness and strength.
Keywords: Reverse bending method | CTOD test | Pre-crack straightness | Residual stress | Welded structure
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1
Crossref
972
View
14
Download
Related articles
A study on the prediction of the angular distortion in line heating with high frequency induction heating   2015 February;33(1)
A Study on Prediction of Fatigue Life using MFC Sensors  2013 December;31(6)
A study on the prediction of the angular distortion in line heating with high frequency induction heating   2015 February;33(1)
A Study on Prediction of Fatigue Life using MFC Sensors  2013 December;31(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.