Characterization of resistance spot welded Al5052/DP590 dissimilar materials and processing optimization
Beom-Ji Jo*,**, Ji-Sun Kim**, Hyo-Sang Yoo**, In-Ju Kim**, Seong-Hui Lee*, Young-Gon Kim**
*Dept. of Advanced Materials Science & Engineering, Mokpo University, Mokpo 534-729, Korea
**Korea Institute of Industrial Technology, Gwangju 500-460, Korea
Correspondence: Young-Gon Kim  Email: ygkim1@kitech.re.kr
  Published online April 30, 2015
ABSTRACT
IRW(Inverter Resistance Welding) process and DSW(Delta-spot welding) process for dissimilar materials of DP590 and Al5052 were performed to evaluate the welding quality and mechanical properties. IRW experiment was carried out with changing the welding current. The other welding parameters such as pressure force, weld time, squeezing time and holding time were fixed. On the anther hand, DSW experiment was performed using the process tape at welding current of 11.5kA. The other conditions were same as IRW conditions. The various testes such as shear tensile strength, nugget diameters, EDS, SEM and cross-sectional observation for weld zone was performed. As a result, IMC(Inter Metallic Compound) thickness at 11.5kA was thinner than those of 9.5kA and 10.5kA conditions. In addition, thined IMC layer was observed when high electric current apply to the materials(DP590 and Al5052) in a short time throught dissimilar resistance spot welding controling welding conditions. The relationship between the thickeness of IMC and current intensity was after discussed.
Keywords: Intermetallic compound | DP590 | Al5052 | Shearing stress | Weld nugget | Resistance spot welding | Delta-Spot welding
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
3
Crossref
1,210
View
13
Download
Related article
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.