Numerical analysis on the welding residual stress and fracture toughness of the heavy thick steel welded joints by welding processes
HanSur Bang*, HeeSeon Bang*
*Department of Welding and Joining Science Engineering, Chosun University, Gwangju 501-759, Korea
Correspondence: HeeSeon Bang  Email: banghs@chosun.ac.kr
  Published online April 30, 2015
ABSTRACT
This study examined the welding residual stress and fracture toughness of 78mm thick steel electro gas welding (EGW) and flux cored arc welding (FCAW) welded joints by numerical analyses of the thermal elasto-plastic behavior and fracture toughness(KIC). The residual stress, fracture toughness characteristics and production mechanism on the welded joints were clarified. Moreover, the effects of the welding process (EGW and FCAW) on the welding residual stresses and fracture toughness of welded joints were evaluated. The results showed that the new welding process (EGW) appears to be an effective substitute for the existing welding process (FCAW) in a thick steel plate with high strength.
Keywords: Heavy thick steel; Electro gas welding (EGW); Flux cored arc welding (FCAW); Welding residual stress; Fracture toughness
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,203
View
5
Download
Related articles
Numerical Analysis of Welding Residual Stresses for Ultra-thick Plate of EH40 TM and API 2W Gr.50 Steel Joined by Flux Core Arc Welding  2010 June;28(3)
The Analysis of the Residual Stress and Bending Characteristies on the Heterogeneous Materials by Laser Welding  2004 June;22(3)
Numerical Analysis of Welding Residual Stresses for Ultra-thick Plate of EH40 TM and API 2W Gr.50 Steel Joined by Flux Core Arc Welding  2010 June;28(3)
The Analysis of the Residual Stress and Bending Characteristies on the Heterogeneous Materials by Laser Welding  2004 June;22(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.