Evaluation HIC Crack Resistance for Plastic Deformation of API-X65 Plate
Hoi-Soo Ryoo*, Jun Seok Seo*, Hee-jin Kim*, Dong-Eon Lee**
*Korea Institute of Industrial Technology, Advanced Welding & Joining R&D Group
**SeAH Steel Corp., Technical Research Institute New Material Research
Correspondence: Hoi-Soo Ryoo  Email: hsryoo@kitech.re.kr
  Published online December 23, 2012
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
857
View
5
Download
Related articles
Evaluation of Fracture Safety According to Plastic Deformation with High Strength Steel Weld Joints  2019 December;37(6)
Evaluation on Resistance Spot Weldability and Nugget Formation of Surface Roughness Treated Steel Sheet  2008 October;26(5)
Evaluation of HIC Resistance for Thick-wall Welded Pipe  2005 June;23(3)
Evaluation of Fracture Safety According to Plastic Deformation with High Strength Steel Weld Joints  2019 December;37(6)
Evaluation on Resistance Spot Weldability and Nugget Formation of Surface Roughness Treated Steel Sheet  2008 October;26(5)
Evaluation of HIC Resistance for Thick-wall Welded Pipe  2005 June;23(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.