The Effect of Fatigue Strength according to Carburizing Depth
Hyun Min Choi*, Yong Ha Park**, Yong Taek Shin***, Myung Hyun Kim*
*Dept. of Naval Architecture and Ocean Engineering, Pusan National University, Busan 609-735, Korea
**Dept. of Materials Research, Samsung Heavy Industries Co., Ltd, Geoje-si, Gyungnam 656-710, Korea
***Dept. of Materials Science and Engineering, Donga University, Busan 604-714, Korea
Correspondence: Myung Hyun Kim  Email: kimm@pusan.ac.kr
  Published online August 30, 2014
ABSTRACT
Carburizing treatments are the important way to developing fatigue strength and wear resistance. It is well known that the case depth is one of the most significant parameters determining fatigue strength. In this study, 3-point bending fatigue test was conducted to evaluate fatigue strength for the carburized depth with 18CrNiMo7-6 steel. As a result, fatigue strength increased with effective case depth decreased. It is shown that hardness in case hardened layer played principal role in the fatigue strength.
Keywords: Fatigue strength | 3-Point bending fatigue test | Carburized steel
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,258
View
9
Download
Related articles
Review of Fatigue Strength Evaluation on Weld Joints of Hull Structure   1994 September;12(3)
The Effect of Carbon Content on Hot Cracking of Low Carbon Steel Weld   1988 December;6(4)
Review of Fatigue Strength Evaluation on Weld Joints of Hull Structure   1994 September;12(3)
The Effect of Carbon Content on Hot Cracking of Low Carbon Steel Weld   1988 December;6(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.