Numerical Studies on Submerged Arc Welding Process |
Degala Ventaka Kiran*, Suck-Joo Na* |
*Department of Mechanical Engineering, KAIST, Daejeon 305-701, Korea |
Correspondence:
Suck-Joo Na Email: sjoona@kaist.ac.kr Published online August 30, 2014
|
|
|
A quantitative understanding on the effect of the welding conditions on weld joint dimensions and weld thermal cycle is difficult through experimental studies alone. The experimental realization of temperature distribution in the weld pool is proved to be extremely difficult due to the small size of welds, high peak temperature and steep temperature gradients in weld pool. This review deals with the heat transfer and fluid flow analysis to understand the parametric influence of a single wire submerged arc welding (SAW) and multi-wire SAW processes on the weld bead dimensions, temperature and fluid flow distribution in the weldment. |
Keywords:
Submerged arc welding process | Heat transfer and fluid flow analysis | Tandem submerged arc welding process.
|
|
|
|
|
 |
|
|
 |
Register for e-submission |
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
|
Manuscript Submission |
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
|
Free archive |
Anyone may access any past or current articles without logging in.
|
|
|