A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding
Yong-Rae Kim*, Gyu-Yeong Song**, Chao Wang***, Jae-Woong Kim***
*Dept. of Mechanical Engineering, Graduate School of Yeungnam University, Kyongsan-Kyongbuk 721-749, Korea
**Kyongbuk Hybrid Technology Institute, Yeongcheon-Kyongbuk 770-170, Korea
***School of Mechanical Engineering, Yeungnam University, Kyongsan-Kyongbuk 721-749, Korea
Correspondence: Jae-Woong Kim  Email: jaekim@ynu.ac.kr
  Published online January 21, 2014
ABSTRACT
The welding distortion is caused by welding heat in the structures which are widely used in shipbuilding and automotive industries, thus many researchers have proposed such methods to control the welding distortion through trials and numerical studies. The welding distortion has been the main cause of low productivity due to the structural strength degradation, apparent flaw, additional deformation caused by the process followed the current assembly step, and the increase of correction workload. The deformation of fillet welding is investigated in this study, and the influence of the rib height on the welding distortion is verified through the actual experiment. And the numerical analysis model using the FE software MSC.marc for analysis of welding distortion is proposed.
Keywords: Welding distortion | Longitudinal bending | Angular distortion | Finite element analysis
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,366
View
9
Download
Related articles
A Study on Deformation According to Welding Speed of Root Pass in GTAW Butt Joint Welding  2019 October;37(5)
A Study on the Estimation of Weld Quality Using the Thermal Images During Arc Welding  2018 February;36(1)
Study on the Welding Mode Transition Phenomena in Monitoring Plasma-MIG Hybrid Welding   2017 June;35(3)
A study on the prediction of the angular distortion in line heating with high frequency induction heating   2015 February;33(1)
A Study on the Thermal Distortion Analysis of Welded Structures having K/X Groove using shell elements  2012 December;30(6)
A Study on Deformation According to Welding Speed of Root Pass in GTAW Butt Joint Welding  2019 October;37(5)
A Study on the Estimation of Weld Quality Using the Thermal Images During Arc Welding  2018 February;36(1)
Study on the Welding Mode Transition Phenomena in Monitoring Plasma-MIG Hybrid Welding   2017 June;35(3)
A study on the prediction of the angular distortion in line heating with high frequency induction heating   2015 February;33(1)
A Study on the Thermal Distortion Analysis of Welded Structures having K/X Groove using shell elements  2012 December;30(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.