A Study on Prediction of Fatigue Life using MFC Sensors
Ji-Hoon Lee, Dong-Jin Oh, Myung-Hyun Kim
Dept. of Naval Architecture and Ocean Engineering, Pusan National University, Busan 609-735, Korea
Correspondence: Myung-Hyun Kim  Email: kimm@pusan.ac.kr
  Published online January 21, 2014
ABSTRACT
The large-scale structures have the possibility that there are defects such as cracks due to stress concentration caused by geometric discontinuities in the structure. In this respect, the assessment of fatigue life and the development of structural health monitoring(SHM) are very important. Fatigue design of structure is typically accomplished either using a set of stress cycle (S-N) data obtained from fatigue tests or using the fracture mechanics approach. The stress intensity factor(SIF) is required for the estimation of fatigue crack propagation life from the linear elastic fracture mechanics (LEFM) perspective. In this study, Macro Fiber Composie(MFC) sensor for the measurement of SIF of two dimensional cracks is used. The SIF based on the piezoelectric constitutive law and fracture mechanics are calculated. The measured values of the SIF are later used for the prediction of the crack propagation life. In this study, the measured value of the SIF and the fatigue life are compared with the theoretical results.
Keywords: MFC sensor | Stress intensity factor(SIF) | Fatigue crack propagation life
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,160
View
4
Download
Related articles
A Study for Brittle Crack Prevention and Fatigue Life Improvement using a Welded Stiffener  2018 December;36(6)
A study on reduction of pre-crack deviation in CTOD specimen using reverse bending method  2015 April;33(2)
A Study on Bead Geometry Prediction the GMA Fillet Welding using Genetic Algorithm  2012 December;30(6)
A Study of the Effect of Magnetic Fields Using Welding Process  2014 October;32(5)
A Study on the Evaluation of Fatigue Strength of Welded Lap Joint with Element Stress Approach  2014 February;32(1)
A Study for Brittle Crack Prevention and Fatigue Life Improvement using a Welded Stiffener  2018 December;36(6)
A study on reduction of pre-crack deviation in CTOD specimen using reverse bending method  2015 April;33(2)
A Study on Bead Geometry Prediction the GMA Fillet Welding using Genetic Algorithm  2012 December;30(6)
A Study of the Effect of Magnetic Fields Using Welding Process  2014 October;32(5)
A Study on the Evaluation of Fatigue Strength of Welded Lap Joint with Element Stress Approach  2014 February;32(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.