VHCF Characteristics of SCMH2 Steel Depending on the Surface Treatment Conditions
C.M. Suh1, C.H. Suh2, M.S. Suh3
1School of Mechanical Engineering, Kyungpook National University, Daegu 702-701 Korea
2Daegu Mechatronics & Materials Institute, Daegu 704-240 Korea
3Korea Institute of Energy Research, Daejeon, 305-343 Korea
Correspondence: M.S. Suh  Email: mssuh@kier.re.kr
  Published online August 31, 2013
ABSTRACT
SCMH2 steel is widely used in the industrial members of car and tractor. This study focused on material properties and evaluation technology of the SCMH2 steel regarding the surface treatment followed by carburizing and nitriding, by means of impact test, hardness test. and fatigue test including HCF (high cycle fatigue) and VHCF (very high cycle fatigue). Drop weight impact tester (Instron, 9250 Hv) and Cantilever type rotating-bending fatigue tester (YRB200, 3150 rpm) were used to characterize the SCMH2 standard specimen before and after carburizing/nitriding. In order to understand those effects on fatigue characteristics and material properties, the fractured surfaces were carefully observed and analyzed by SEM (scanning electron microscope) and EDS (energy-dispersive X-ray spectroscopy).
Keywords: SCMH2 | VHCF(Very High Cycle Fatigue) | Impact | Carburizing | Nitriding
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,257
View
3
Download
Related articles
Fracture Characteristics of Cryogenic Steel Using Weibull Stress Analysis  2019 December;37(6)
Study on the Corrosion Resistance of High Strength Bolt, Nut and Washer Set (S10T) Related to the Surface Treatment Conditions  2018 April;36(2)
A Study on the Characteristics of Laser Deposition Surface and Cross-section for Metal Powder  2016 August;34(4)
Characteristics of Organic Coated Steel Strip and the Joining Technique  2008 June;26(3)
Characteristics of Cut Surface by Abrasive Waterjet Cutting of Titanium Alloy  2005 February;23(1)
Fracture Characteristics of Cryogenic Steel Using Weibull Stress Analysis  2019 December;37(6)
Study on the Corrosion Resistance of High Strength Bolt, Nut and Washer Set (S10T) Related to the Surface Treatment Conditions  2018 April;36(2)
A Study on the Characteristics of Laser Deposition Surface and Cross-section for Metal Powder  2016 August;34(4)
Characteristics of Organic Coated Steel Strip and the Joining Technique  2008 June;26(3)
Characteristics of Cut Surface by Abrasive Waterjet Cutting of Titanium Alloy  2005 February;23(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.