Effects of the Types of Coating on the Laser Brazing Characteristics of Dissimilar Joints between Mg Alloy and Steel Sheet
Mok-Young Lee1, Sook-Whan Kim2, ALI M. NASIRI3, NORMAN Y. ZHOU3
1Advanced Metallic Materials Research Department, RIST, Pohang 790-330, Korea
2Energy Infra Research Department, RIST, Pohang 790-330, Korea
3Department of Mechanical & Mechatronics Engineering, University of Waterloo, Waterloo, ON, N2L 3G1, Canada
Correspondence: Mok-Young Lee  Email: accelee@rist.re.kr
  Published online August 31, 2013
ABSTRACT
The dissimilar welding between magnesium alloy and steel sheet was required in automobile industry to increase the strength of the dissimilar joints. Laser brazing is one of the good joining processes for Mgsteel dissimilar joint. In this study, the effect of coating materials was evaluated on the laser brazing for the dissimilar joint between AZ31 and coated steels such as Zn, Sn and Ni. Diode direct laser was used to braze the lap-edge joint with Mg600 filler wire and Superior #21 flux. The wettability was best on Zn coated steel. The interlayer was formed at the interface between brazement and steel for all coating materials. The strengths of brazed specimen were 146.5N/mm, 204.6N/mm and 101.6N/mm for Zn, Sn and Ni coated steel respectively.
Keywords: Mg alloy | Dissimilar joint | Coated steel sheet | Laser brazing | Diode direct laser
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,174
View
4
Download
Related articles
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding  2017 October;35(5)
Effect of B Contents on Hardness Characteristic of Disk Laser Beam Welded CP Steels  2011 February;29(1)
Effect of He Mixing Ratio on the Characteristic of TIG Welding with High Current and High Speed  2005 June;23(3)
The Effects of Heat-treatment on Brazing Characteristics of WC-9%Co/SUJ2 Steel   1997 October;15(5)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding  2017 October;35(5)
Effect of B Contents on Hardness Characteristic of Disk Laser Beam Welded CP Steels  2011 February;29(1)
Effect of He Mixing Ratio on the Characteristic of TIG Welding with High Current and High Speed  2005 June;23(3)
The Effects of Heat-treatment on Brazing Characteristics of WC-9%Co/SUJ2 Steel   1997 October;15(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.