Measurement of Weld Mechanical Properties of SUS316L Plate Using an Instrumented Indentation Technique
Kee-Nam Song, Sung-Deok Hong, Dong-Seong Ro
Nuclear Hydrogen Reactor Technology Development Division, KAERI, Daejeon 305-353, Korea
Frontics Ltd., Seoul 153-704, Korea
Correspondence: Kee-Nam Song  Email: knsong@kaeri.re.kr
  Published online June 5, 2013
ABSTRACT
Different microstructures in the weld zone of a metal structure such as a fusion zone or heat affected zone are formed as compared to the parent material. Thus, the mechanical properties in the weld zone are different from those in the parent material. As the basic data for reliably understanding the structural characteristics of welded PCHE prototype made of SUS316L, the mechanical properties in the weld zone and parent material for a SUS316L plate are measured using an the instrumented indentation technique in this study.
Keywords: Instrumented indentation technique | Mechanical property | PCHE(Printed Circuited Heat Exchanger) | very high temperature reactor
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
6
Crossref
1,433
View
14
Download
Related articles
A Study on the Mechanical Properties of Heated Plates by Induction Heating System  2014 February;32(1)
Measurement of Weld Material Properties of Alloy 617 Using an Instrumented Indentation Technique  2013 October;31(5)
Development of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Invar 42/SS 400  2012 October;30(5)
Measurement of Mmechanical Properties in Weld Zone of Nuclear Material using an Instrumented Indentation Technique  2012 June;30(3)
Evaluation of Residual Stress on Welded Joint in API X65 Pipe Line through Nondestructive Instrumented Indentation Technique  2003 September;21(5)
A Study on the Mechanical Properties of Heated Plates by Induction Heating System  2014 February;32(1)
Measurement of Weld Material Properties of Alloy 617 Using an Instrumented Indentation Technique  2013 October;31(5)
Development of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Invar 42/SS 400  2012 October;30(5)
Measurement of Mmechanical Properties in Weld Zone of Nuclear Material using an Instrumented Indentation Technique  2012 June;30(3)
Evaluation of Residual Stress on Welded Joint in API X65 Pipe Line through Nondestructive Instrumented Indentation Technique  2003 September;21(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.