ABSTRACT
  Butt-joints of A6061-T6 and AZ31 plates were successfully manufactured by using a friction stir welding method. Off-set free joints and off-set joints were fabricated to investigate the effect of the tool plunge position on the mechanical properties of the joints. Hardness test, tensile test and charpy impact test was performed to evaluate the mechanical properties of the joints. Off-set condition resulted in increase of mechanical properties of the joints. The variation of the hardness distribution in the SZ was also stabilized in the off-set condition. Tensile strength of the off-set joint was about 85% against to that of the AZ31 base metal. Impact absorption energy by Charpy-Impact-Test of the off-set joint also increased by almost 2 times against to that of the AZ31 base metal.
Keywords: Friction stir welding;Tool plunge position;Mechanical properties;A6061-T6;AZ31
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,469
View
0
Download
Related articles
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars  2019 February;37(1)
Heat Transfer Simulation and Effect of Tool Pin Profile and Rotational Speed on Mechanical Properties of Friction Stir Welded AA5083-O  2017 June;35(3)
Effects of High Temperature-moisture on Corrosion and Mechanical Properties for Sn-system Solder Joints   2017 June;35(3)
Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint  2016 June;34(3)
Evaluation of mechanical properties on friction stir lap jointed Al6061/HT590 alloys  2015 April;33(2)
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars  2019 February;37(1)
Heat Transfer Simulation and Effect of Tool Pin Profile and Rotational Speed on Mechanical Properties of Friction Stir Welded AA5083-O  2017 June;35(3)
Effects of High Temperature-moisture on Corrosion and Mechanical Properties for Sn-system Solder Joints   2017 June;35(3)
Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint  2016 June;34(3)
Evaluation of mechanical properties on friction stir lap jointed Al6061/HT590 alloys  2015 April;33(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.