The Effect of Welding Condition on Tensile Properties of Friction Stir Welds of KS5J32 Al Alloy
Tae-Jin Yoon, Sang-Ju Kim, Nam-Kyu Kim, Sang-Woo Song, Chung-Yun Kang




Correspondence:   Published online November 22, 2011
ABSTRACT
  The effect of welding condition on tensile properties of KS5J32 Al Alloy was investigated under various welding conditions. The 1.6 mm thick KS5J32 alloy sheets were joined by friction stir welding (FSW) technique with butt joint. The tool rotation speeds were 1000, 1250 and 1500 rpm, and the welding speeds were varied within the range from 100 to 600 ㎜/min. Voids mainly occurred at the advancing side of the tool probe, when the tool rotation speed was low, due to insufficient materials flow. When the weld pitch exceeded 0.4 ㎜/rev, voids were observed under all welding conditions and the area of voids increased with increasing weld pitch. For void-free specimens, fracture always occurred at base materials. However voids affected the location of fractures, base metal or welded zone, when the voids existed within the welds.
Keywords: Friction stir welding;A5023;KS5J32;Weld pitch
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,312
View
0
Download
Related articles
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars  
Influence of Workpiece Tilting Angle on Joint Properties in Tailor Friction Stir Welded Blanks of Aluminium Alloy 5052-H32  2018 October;36(5)
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   2017 August;35(4)
Heat Transfer Simulation and Effect of Tool Pin Profile and Rotational Speed on Mechanical Properties of Friction Stir Welded AA5083-O  2017 June;35(3)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars   ;0(0)
Influence of Workpiece Tilting Angle on Joint Properties in Tailor Friction Stir Welded Blanks of Aluminium Alloy 5052-H32  2018 October;36(5)
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   2017 August;35(4)
Heat Transfer Simulation and Effect of Tool Pin Profile and Rotational Speed on Mechanical Properties of Friction Stir Welded AA5083-O  2017 June;35(3)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.