A Study on the Optimum Line Heating Condition for Straightening a Thin Plate Welded Structure
Jun-Hyoung Park, Jae-Woong Kim

Correspondence:   Published online May 7, 2011
ABSTRACT
  The purpose of this study is to establish the optimum line heating condition to straighten the excessive bending distortion of a thin plate welded structure. For it, the extensive FEA and experiments were performed to evaluate the effect of heat source, heating speed and position on the straightening of a thin plate welded structure. In accordance with the results obtained by FEA and experiments, the straightening effect of line heating was strongly depends on the variables used in this study. With the results, the optimum line heating condition was established by using the response surface method and verified through comparing it with the numerical analysis result.
Keywords: : Line heating straightening;Sheet metal;Weld distortion;Numerical analysis;Finite element method(FEM);Optimal condition
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,048
View
0
Download
Related articles
A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding  2013 December;31(6)
A Study on Weldment Boundary Condition for Elasto-Plastic Thermal Distortion Analysis of Large Welded Structures  2011 August;29(4)
A Experiment Study for Selection of Welding Condition of fillet Welded Structure  2011 August;29(4)
A Study on the Weld-induced Residual Stress Analysis at FPSO Moon Pool Structure  2011 June;29(3)
A Study on the Prediction of the Optimal Welding Condition for Automotive Steel Sheets in MAG Welding Process  2009 June;27(3)
A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding  2013 December;31(6)
A Study on Weldment Boundary Condition for Elasto-Plastic Thermal Distortion Analysis of Large Welded Structures  2011 August;29(4)
A Experiment Study for Selection of Welding Condition of fillet Welded Structure  2011 August;29(4)
A Study on the Weld-induced Residual Stress Analysis at FPSO Moon Pool Structure  2011 June;29(3)
A Study on the Prediction of the Optimal Welding Condition for Automotive Steel Sheets in MAG Welding Process  2009 June;27(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.