Effects of Outside Repair Welding on the Crack Growth in the Surge Nozzle Weld on the Hot Leg Side in a Nuclear Power Plant
Kyung-Hwan Na, Eunsub Yun, YoungSheop Park


Correspondence:   Published online May 7, 2011
ABSTRACT
  Nickel-based austenitic alloys such as Alloy 82 and 182 had been employed as the weld metals in nuclear power plants (NPPs) due to their high corrosion resistance as well as good mechanical properties. However, since the 2000s, the occurrence of primary water stress corrosion cracking has been reported in conjunction with these alloys in domestic and oversea NPPs. In the present work, we assumed an imaginary crack at the inner surface of a surge nozzle weld that had previously experienced the outside repair welding, and constructed its finite element model. Finite element analysis was performed with respect to the heat transfer, and then to the residual stress for obtaining the total applied stress distributions. These stress distributions were finally converted to the stress intensity factors for estimating crack growth rate. From the comparison of crack growth rate curves for the cases of no repair welding and outside repair welding, it was found that the outside repair welding did not exhibit negative effect on the crack growth for the surge nozzle under consideration in this work; in both cases, the cracks stopped growing before they became the through-wall cracks.
Keywords: Dissimilar metal weld;Repair welding;PWSCC;Alloy 82/182
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
859
View
0
Download
Related article
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.