Microtexture and Material Flow Analysis on Friction Stir Welded Materials
SukHoon Kang, Jae-Hyung Cho, ChangGil Lee, Sung-Joon Kim, KyuHwan Oh, HeungNam Han





Correspondence:   Published online November 5, 2010
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
973
View
0
Download
Related articles
Microstructure and Phase Analysis of Pure Ti and Ti-6Al-4V GTAW Cladding Material  2020 April;38(2)
Microtexture and Microstructural Evolution of Friction Stir Welded AA5052-H32 Joints  2019 April;37(2)
Microstructure and Mechanical Properties in the Friction Stir Welded C70600 Alloy  2018 April;36(2)
Recent Trends of Friction Stir Welding of Titanium  2013 April;31(2)
Development of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Invar 42/SS 400  2012 October;30(5)
Microstructure and Phase Analysis of Pure Ti and Ti-6Al-4V GTAW Cladding Material  2020 April;38(2)
Microtexture and Microstructural Evolution of Friction Stir Welded AA5052-H32 Joints  2019 April;37(2)
Microstructure and Mechanical Properties in the Friction Stir Welded C70600 Alloy  2018 April;36(2)
Recent Trends of Friction Stir Welding of Titanium  2013 April;31(2)
Development of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Invar 42/SS 400  2012 October;30(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.