Development of Monitoring Process of Friction Stir Spot Welding of Aluminum Alloys using Acoustic Emission
Yong-Wook Lee, Hak-Chun Lee, Jong-Whan Park, Kyu-Yeol Park, Sung-Tae Hong, Jae-Hyun Hwang





Correspondence:   Published online November 5, 2010
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
833
View
0
Download
Related articles
Influence of Workpiece Tilting Angle on Joint Properties in Tailor Friction Stir Welded Blanks of Aluminium Alloy 5052-H32  2018 October;36(5)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint  2016 June;34(3)
Researches in Corrosion Resistance of Friction Stir Welded Aluminum alloys  2013 April;31(2)
Recent Developments in Friction Stir Welding Technology of Stainless Steels  2012 October;30(5)
Influence of Workpiece Tilting Angle on Joint Properties in Tailor Friction Stir Welded Blanks of Aluminium Alloy 5052-H32  2018 October;36(5)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint  2016 June;34(3)
Researches in Corrosion Resistance of Friction Stir Welded Aluminum alloys  2013 April;31(2)
Recent Developments in Friction Stir Welding Technology of Stainless Steels  2012 October;30(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.