ABSTRACT
  The purpose of this paper is to understand the behavior of GHTAW process under the space environment with the experimental and numerical analysis. Gas Hollow Tungsten Arc Welding (GHTAW) using a hollow tungsten electrode was adopted, since the ignition and discharge of a conventional GTAW process is not appropriate to the space environment due to low pressure in space. In order to clarify the phenomena of GHTAW under space environment, an investigation of thermal and physical properties of the GHTAW arc plasma was experimentally performed under low pressure conditions. Furthermore, the molten pool behavior and weldment of GHTAW were understood by CFD-based numerical analysis, based on the models of GHTA heat source, arc pressure and electromagnetic force induced by arc plasma, the characteristics of which were obtained by the captured images of a CCD camera.
Keywords: GHTAW;Arc plasma;Numerical simulation;Heat source;Modeling;Space welding;Molten pool
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
983
View
0
Download
Related articles
A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(I) - Characteristic Analysis of One-pass Clad Layer with Parameters -  2018 December;36(6)
A Study on the Crash Characteristics and Analysis of Spot+adhesive Welds in Automobile B-pillar Parts  2011 October;29(5)
A Study on the High Temperature Tensile Characterisitics of Lap Weld of 15Cr Ferritic Stainless Steels  2008 October;26(5)
A Study on the Adhesive Characteristics of Nano Scale Particles Considering Asperity Interaction  2008 February;26(1)
A Study on the Strength Characteristics of Welded Joints in Aluminum Carbody of Rolling Stock  2005 February;23(1)
A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(I) - Characteristic Analysis of One-pass Clad Layer with Parameters -  2018 December;36(6)
A Study on the Crash Characteristics and Analysis of Spot+adhesive Welds in Automobile B-pillar Parts  2011 October;29(5)
A Study on the High Temperature Tensile Characterisitics of Lap Weld of 15Cr Ferritic Stainless Steels  2008 October;26(5)
A Study on the Adhesive Characteristics of Nano Scale Particles Considering Asperity Interaction  2008 February;26(1)
A Study on the Strength Characteristics of Welded Joints in Aluminum Carbody of Rolling Stock  2005 February;23(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.