JWJ > Volume 28(4); 2010 > Article
Journal of KWJS 2010 August;28(4) :9-13.
Published online September 8, 2010.
The Study on Radiation Source Optimization for Boiler Tube Weldments
Sang-Ki Park, Yean-Shic Ahn, Doo-Song Gil


Correspondence:   Published online September 8, 2010
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
792
View
0
Download
Related articles
Fuzzy Logic Optimization for Low Sulphur and Phosphorus in Submerged Arc Weldments  2017 December;35(6)
A Study on Development of the Optimization Algorithms to Find the Seam Tracking  2016 April;34(2)
Recent Study in Variation of Welding Materials for Overlay Welding  2013 December;31(6)
A Study on Welding Distortion and Residual Stress for Tubular Welded Joint  2012 October;30(5)
A Study on the Optimum Line Heating Condition for Straightening a Thin Plate Welded Structure  2011 April;29(2)
Fuzzy Logic Optimization for Low Sulphur and Phosphorus in Submerged Arc Weldments  2017 December;35(6)
A Study on Development of the Optimization Algorithms to Find the Seam Tracking  2016 April;34(2)
Recent Study in Variation of Welding Materials for Overlay Welding  2013 December;31(6)
A Study on Welding Distortion and Residual Stress for Tubular Welded Joint  2012 October;30(5)
A Study on the Optimum Line Heating Condition for Straightening a Thin Plate Welded Structure  2011 April;29(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.