ABSTRACT
  High Mn steel has been developed for automotive applications since the steel has an excellent combination of strength and ductility. However, from the viewpoint of welding, high Mn steel has a few problems related to its chemical composition. This paper describes characteristics of dissimilar CO₂ laser welding for expanding application of high Mn steel. From this work it was cleared that dissimilar laser welded joint between high Mn steel and carbon steel had poor formability due to the formation of martensite within weld metal. In order to improve ductility of welded joint, the method of controlling the dilution ratio of high Mn steel was suggested.
Keywords: High Mn steel;CO₂ Laser welding;Dissimilar welding;Formability
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,168
View
0
Download
Related articles
Characteristic of Welding Rotational Deformation in Laser Welding of Thin Steel Sheet  2018 December;36(6)
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input  2018 June;36(3)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
Hardness Estimation of Laser Welded Boron Steel Welds with the Carbon Equivalent  2016 October;34(5)
A Study on HAZ Softening Characteristics of Fiber Laser Weldment for High-Strength Steel   2015 December;33(6)
Characteristic of Welding Rotational Deformation in Laser Welding of Thin Steel Sheet  2018 December;36(6)
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input  2018 June;36(3)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
Hardness Estimation of Laser Welded Boron Steel Welds with the Carbon Equivalent  2016 October;34(5)
A Study on HAZ Softening Characteristics of Fiber Laser Weldment for High-Strength Steel   2015 December;33(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.