The Study about Characteristics of Welding Consumable and Weld Metal for EGW
Jeong-Soo Lee, Jin-Oh Yun, Sang-Hoon Jeong, Chul-Gyu Park, Young-Ho An




Correspondence:   Published online May 13, 2010
ABSTRACT
  In this study, newly developed welding consumables for EGW were welded in EH 36 TM steel plates and their welded joints were evaluated in point of mechanical properties and microstructures compared with imported consumables. Newly developed welding consumables were evaluated as good arc stability and slag fluidity, substantially the same with imported products. The tensile strength of all welded joints were sufficient to meet the requirements specified in a ship’s classification(490~640㎫) and all areas of fracture were heat affected zone(HAZ). Charpy absorbed energy values of all EG welded metals were sufficient to meet the requirements of classification(min. 34J) and those of newly developed wires were evaluated to be better than those of imported wires. As a result observing microstructures of single and tandem EG welded metals through optical and scanning electron microscope (OM&SEM), no grain boundary ferrite(PF(G)) were created in a prior austenite grain boundary and a volume fraction of a fine acicular ferrite were observed very high.
Keywords: Welding consumable for EGW;Large hea input;Toughness
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,475
View
0
Download
Related articles
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
Statistical Analysis of World Welding Consumables Market (II)  2019 August;37(4)
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding  2017 October;35(5)
A Study of Characteristics of Vertical-up SMA Welding by Short Circuit Control  2017 October;35(5)
A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW  2017 August;35(4)
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
Statistical Analysis of World Welding Consumables Market (II)  2019 August;37(4)
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding  2017 October;35(5)
A Study of Characteristics of Vertical-up SMA Welding by Short Circuit Control  2017 October;35(5)
A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW  2017 August;35(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI