Influence of Welding Residual Stress on the Mechanical Behavior of Externally Loaded Dissimilar SS400-STS304 Steel Weldment
Hee-Seon Bang, Han-Sur Bang, You-Chul Kim, SungMin Joo, Soon-Won Joa, Chan-Seoung Ro





Correspondence:   Published online November 16, 2009
ABSTRACT
  Thermal and mechanical characteristics in dissimilar SS400-STS304 steel weldment have been investigated by 3D thermal elastic-plastic analysis. Moreover, the influence of welding residual stresses on the mechanical behaviour of this welded joint, by applying superimposed external load (tension load) was determined. The residual stresses obtained by numerical simulation were compared with the experimentally measured results. The FE results were in good agreement with the measured values. The mechanical test (hardness, tensile test) and metallurgical analysis was carried out to ensure the weld integrity. Hence, possibility of applying SS400-STS304 dissimilar steels in industries has been established.
Keywords: Dissimilar SS400-STS304 steel weldment;3D thermal elastic-plastic analysis;Welding residual stress;External load
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
928
View
0
Download
Related articles
Analysis of Welding Residual Stress Redistributions on Notched Multi-pass FCA Butt Weldment  2010 February;28(1)
Influence of Welding Residual Stress on the Externally Loaded Welded Structure  2007 December;25(5)
Effect of Welding Residual Stress on Fatigue Crack Propagation Behavior   1997 June;15(3)
The influence of post weld heat treatment on mechanical properties of stainless steel weldment   1996 June;14(3)
Effect of PWHT and Stress Ratio on Fatigue Behavior of Welded Joints in Steel   1987 September;5(3)
Analysis of Welding Residual Stress Redistributions on Notched Multi-pass FCA Butt Weldment  2010 February;28(1)
Influence of Welding Residual Stress on the Externally Loaded Welded Structure  2007 December;25(5)
Effect of Welding Residual Stress on Fatigue Crack Propagation Behavior   1997 June;15(3)
The influence of post weld heat treatment on mechanical properties of stainless steel weldment   1996 June;14(3)
Effect of PWHT and Stress Ratio on Fatigue Behavior of Welded Joints in Steel   1987 September;5(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.