Advanced Search  
JWJ > Volume 27(5); 2009 > Article
Journal of KWJS 2009 October;27(5) :1-4.
Published online November 16, 2009.
Laser Welding Characteristics of Ultra High Strength Steel for Automotive Application
Jinkang Choi, Minjung Kang, Jungho Cho, Cheolhee Kim



Correspondence:   Published online November 16, 2009
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
950
View
0
Download
Related articles
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input  2018 June;36(3)
Strength Estimation Model of Resistance Spot Welding of 1.2GPa Grade Ultra High Strength TRIP Steel for Car Body Applications  2018 February;36(1)
Development Trend and Prospect for Improving Fatigue Performance of Advanced High Strength Steel Welds in Automotive Chassis Applications  2017 December;35(6)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input  2018 June;36(3)
Strength Estimation Model of Resistance Spot Welding of 1.2GPa Grade Ultra High Strength TRIP Steel for Car Body Applications  2018 February;36(1)
Development Trend and Prospect for Improving Fatigue Performance of Advanced High Strength Steel Welds in Automotive Chassis Applications  2017 December;35(6)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.