ABSTRACT
  Alloy 600 and Alloy 82/182 materials have been used widely in PWR plants. But these materials are known to be susceptible to PWSCC(Primary Water Stress Corrosion Cracking). Recently, there have been several PWSCC events in major components due to repair welding, because repair welding in the dissimilar metal welds during the construction increases residual stress significantly on the inner surface of welds. In this paper, various residual stress analyses for repair welding were performed using FEM to check the effect of repair welding on residual stress distributions in PZR safety/relief nozzle. The results indicate that for inside surface repair welding, high tensile residual stress is developed on the inside surface of the nozzles.
Keywords: Dissimilar metal weld;PWSCC;Crack;Residual stress;Repair welding
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,088
View
0
Download
Related articles
Statistical Analysis of World Welding Consumables Market (II)  2019 August;37(4)
Statistical Analysis of World Welding Consumables Market  2012 October;30(5)
Recent Studies on Friction Stir Welding Techniques for Dissimilar Materials  2011 October;29(5)
A Study on Machining Effects on Residual Stress at Dissimilar Metal Weld Region  2011 April;29(2)
Crack Growth Analysis of Dissimilar Metal Weld using a Numerical Method  2010 February;28(1)
Statistical Analysis of World Welding Consumables Market (II)  2019 August;37(4)
Statistical Analysis of World Welding Consumables Market  2012 October;30(5)
Recent Studies on Friction Stir Welding Techniques for Dissimilar Materials  2011 October;29(5)
A Study on Machining Effects on Residual Stress at Dissimilar Metal Weld Region  2011 April;29(2)
Crack Growth Analysis of Dissimilar Metal Weld using a Numerical Method  2010 February;28(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.