ABSTRACT
  This research was carried out to improve the productivity in the subassembly process of shipbuilding through optimal work planning for the shortest work time. The work time consist of welding time, moving time of gantry, teaching time of robot and robot motion time. The shortest work time is accomplished by even distribution of work and the shortest welding sequence. Even distribution of work was done by appling the simple algorithm. The shortest work sequence was determined by using GA. The optimal work planning decreased the total work time of the subassembly process by 4.1%. The result showed the effectiveness of the suggested simple algorithm for even distribution of work and GA for the shortest welding sequence.
Keywords: Shipbuilding;Assembly;Genetic algorithm;Even distribution of work;Shortest weldingsequence
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,223
View
0
Download
Related articles
Optimization of Friction Stir Welding Parameters of AA2014-T6 Alloy using Taguchi Statistical Approach  2020 October;38(5)
A Study on Optimization of Fillet in Laser Welding Process for 9% Ni Steel Using Gradient-Based Optimization Algorithm  2020 October;38(5)
Optimization of Weld-bonding Process Conditions of Dissimilar Materials using Delta Spot Welding  2019 June;37(3)
Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method  2018 February;36(1)
Optimization of Process Parameters Using a Genetic Algorithm for Process Automation in Aluminum Laser Welding with Filler Wire  2006 October;24(5)
Optimization of Friction Stir Welding Parameters of AA2014-T6 Alloy using Taguchi Statistical Approach  2020 October;38(5)
A Study on Optimization of Fillet in Laser Welding Process for 9% Ni Steel Using Gradient-Based Optimization Algorithm  2020 October;38(5)
Optimization of Weld-bonding Process Conditions of Dissimilar Materials using Delta Spot Welding  2019 June;37(3)
Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method  2018 February;36(1)
Optimization of Process Parameters Using a Genetic Algorithm for Process Automation in Aluminum Laser Welding with Filler Wire  2006 October;24(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.