Optimization of Robot Welding Process of Subassembly Using Genetic Algorithm in the Shipbuilding |
Ju-Yong Park, Jeong-Jin Seo, Hyun-Jin Kang |
|
Correspondence:
Published online May 18, 2009
|
|
|
This research was carried out to improve the productivity in the subassembly process of shipbuilding through optimal work planning for the shortest work time. The work time consist of welding time, moving time of gantry, teaching time of robot and robot motion time. The shortest work time is accomplished by even distribution of work and the shortest welding sequence. Even distribution of work was done by appling the simple algorithm. The shortest work sequence was determined by using GA. The optimal work planning decreased the total work time of the subassembly process by 4.1%. The result showed the effectiveness of the suggested simple algorithm for even distribution of work and GA for the shortest welding sequence. |
Keywords:
Shipbuilding;Assembly;Genetic algorithm;Even distribution of work;Shortest weldingsequence
|
|
|
|
|
 |
|
|
 |
Register for e-submission |
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
|
Manuscript Submission |
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
|
Free archive |
Anyone may access any past or current articles without logging in.
|
|
|